Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Orgalloy® RS 6630 BLACK - PA66-GF30... - ARKEMA

Material Data Center offers the following functions for Orgalloy® RS 6630 BLACK:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Orgalloy R datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
商品の説明文
Orgalloy® RS 6630 BLACK resin is a fiberglass reinforced polyamide 66 alloy designed for injection molding. This black grade offers an outstanding dimensional stability, chemical resistance to automotive fluids and is ideal for the realization of complex parts.

Main applications:
  • Electric connectors
  • Sport parts
  • Automotive fan shrouds

Packaging:
This grade is delivered dried in sealed packaging (25kg bags) ready to be processed.

Shelf life:
Two years from the date of delivery. For any use above this limit, please refer to our technical services.
Processing/Physical Characteristics乾燥/調湿単位テスト基準
ISO データ
メルトボリュームレイト, MVR 8.5 / * cm³/10min ISO 1133
温度 275 / * °C -
荷重 2.16 / * kg -
機械的特性乾燥/調湿単位テスト基準
ISO データ
引張弾性率 8600 / 8300 MPa ISO 527
破壊応力 129 / 125 MPa ISO 527
破壊ひずみ 2.6 / 3 % ISO 527
引張クリープ弾性率, 1h * / 7900 MPa ISO 899-1
引張クリープ弾性率, 1000h * / 5620 MPa ISO 899-1
シャルピー衝撃強さ, +23°C 58 / 58 kJ/m² ISO 179/1eU
シャルピー衝撃強さ, -30°C 50 / 50 kJ/m² ISO 179/1eU
ノッチ付きシャルピー衝撃強さ, +23°C 10 / 11 kJ/m² ISO 179/1eA
ノッチ付きシャルピー衝撃強さ, -30°C 9 / 9 kJ/m² ISO 179/1eA
ショア硬さD 79 / * - ISO 7619-1
熱的特性乾燥/調湿単位テスト基準
ISO データ
溶融温度, 10°C/min 255 / * °C ISO 11357-1/-3
荷重たわみ温度, 1.80 MPa 237 / * °C ISO 75-1/-2
荷重たわみ温度, 0.45 MPa 257 / * °C ISO 75-1/-2
ビカット軟化温度, B 204 / * °C ISO 306
線膨張係数, 平行 18 / * E-6/K ISO 11359-1/-2
線膨張係数, 直角 110 / * E-6/K ISO 11359-1/-2
1.5mm厚さでの燃焼性 HB / * class IEC 60695-11-10
試験片の厚さ 1.6 / * mm -
厚さhでの燃焼性 HB / * class IEC 60695-11-10
試験片の厚さ 3.2 / * mm -
電気的特性.乾燥/調湿単位テスト基準
ISO データ
比誘電率, 100Hz - / 3 - IEC 62631-2-1
比誘電率, 1MHz - / 4 - IEC 62631-2-1
誘電正接, 100Hz - / 290 E-4 IEC 62631-2-1
誘電正接, 1MHz - / 160 E-4 IEC 62631-2-1
体積抵抗率 - / >1E13 Ohm*m IEC 62631-3-1
表面抵抗率 * / >1E15 Ohm IEC 62631-3-2
耐電圧 34 / 34 kV/mm IEC 60243-1
耐トラッキング性 * / 600 - IEC 60112
その他の特性.乾燥/調湿単位テスト基準
吸水率 3.9 / * % Sim. to ISO 62
吸湿率 1.3 / * % Sim. to ISO 62
密度 1270 / 1270 kg/m³ ISO 1183
Processing Recommendation Injection Molding単位テスト基準
Pre-drying - Temperature 80 °C -
Pre-drying - Time 4 - 8 h -
樹脂温度 270 - 290 °C -
金型温度 60 - 80 °C -
機能
 粘度せん断速度. , Orgalloy® RS 6630 BLACK, PA66-GF30..., ARKEMA
 せん断応力-せん断速度. , Orgalloy® RS 6630 BLACK, PA66-GF30..., ARKEMA
 せん断弾性率-温度. , Orgalloy® RS 6630 BLACK (乾燥), PA66-GF30..., ARKEMA
特殊な特性
成形加工法.
射出成形.
納入形状.
ペレット., 黒
特殊な特性.
光安定化., 熱安定化.
領域別の利用可能性
その他の情報
村遜速揃
Processing conditions:
- Drying time (only necessary for bags opened for more than two hours): 4-8 hours at 80°C
- Injection temperature (min-recommended-max): 270-280-290°C 
- Mould temperature (min-max): 60-80°C 
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.